Aluminium Alloy 2011


Technical Data Sheet

 

Chemical Composition Limits

Weight%

Al

Si

Fe

Cu

Zn

Bi

Pb

Others

2011

Bal

0.40 max

0.70 max

5.0-6.0

0.30 max

0.20-0.60

0.20-0.60

0.05 (each)
0.15 (total)

Aluminium 2011 is a heat treatable high strength alloy with high fatigue strength and excellent free machining characteristics. Due to the high copper content of Alloy 2011 makes it the best choice for aluminium machining. Alloy 2011 is used for screws, bolts, fittings, nuts, automatic lathe and screw machine products.

Provide all grade of these alloy by different shape & size is Our expertise

For any inquiry & request, don't hesitate to contact us

 

Typical Mechanical Properties

 

Material

Temps

Thickness (min)

Tensile Strength (N/mm²) min

Yield Strength (N/mm²) min

Elongation on 50mm (%)

2011 Bar

TD

<10

310

255

6

2011 Bar

TD

10-35

310

255

8

2011 Bar

TD

35-50

295

230

8

2011 Bar

TF

<65

310

225

8

2011 Bar

TF

>65

295

195

8

Specifications
Similar Specifications
BS FC1
Alcoa-800
AWCO-308
BA 308
Durcilium-L
Hiduminium-39
Decoltal-500
QQ-A-225/3

Provide all grade of these alloy by different shape & size is Our expertise

For any inquiry & request, don't hesitate to contact us

Disclaimer
Every effort is made to ensure that technical specifications are accurate. However, technical specifications included herein should be used as a guideline only. All specifications are subject to change without notice.